PP Xim Masterbatch Xaiv Phau Ntawv Qhia

1. Kev faib tawm tseem ceeb

Hom

Yam ntxwv

Daim ntawv thov

Sau ntawv

Txhaj Molding Qib

High dispersion, siab ntws, MI Ntau dua los yog sib npaug rau 20

Txhaj Molding

Khoom siv hauv tsev, khoom ua si, khoom siv

Blown Film Qib

Stretch-resistant, zoo li zaj duab xis

Zaj movie/Nkauj tawm tshiab

Ntim zaj duab xis, woven hnab

Fiber Qib

Tsawg lim tus nqi, siab -temp resistance

Nonwoven / Fiber spinning

Daim npog qhov ncauj, cov khoom siv tu cev

Qib / Ntawv Qib

UV-resistant, siab xim ceev

Extrusion kav / ntawv

Cov khoom siv sab nrauv, cov kav dej

Food Contact Qib

FDA / EU 10/2011 ua raws

Ntim Cov Khoom Noj

Tableware, ntim khoom noj

2. Tsib Txheej Txheem Xaiv Tsa

① Carrier Resin Compatibility

Homopolymer PP puag → Siv homopolymer PP cab kuj masterbatch

Copolymer PP puag → Siv copolymer PP cab kuj masterbatch

Cov khoom siv tsis sib xws ua rau muaj qhov tsis xws luag, xim xim, thiab txo cov khoom siv kho tshuab

② Melt Flow Index (MFI) Matching

MFI ntawm masterbatch yuav tsum ntau dua los yog sib npaug rau hauv paus cob MFI, los yog nyob rau hauv ± 5 g / 10min

Txhaj tshuaj molding: puag resin MFI 10 ~ 30, masterbatch MFI Ntau dua lossis sib npaug rau 20 pom zoo

Fiber spinning: puag ncig MFI 25 ~ 40, masterbatch MFI Ntau dua lossis sib npaug rau 35 pom zoo

③ Pigment Thaum tshav kub kub Resistance

PP ua haujlwm kub: 200 ~ 260℃- pigments yuav tsum nyob ruaj khov

Organic pigments: xaiv cov qib uas muaj cua sov ua haujlwm siab dua lossis sib npaug ntawm 260℃(xws li PR 254, PB 15: 3)

Zam tsis txhob qis- cua sov-kuj azo pigments - nquag hloov xim lossis los ntshav

④ Dispersion Quality

Thov Lim Siab Tus Nqi (DF Tus Nqi) cov ntawv ceeb toom los ntawm cov neeg muag khoom

Qib fiber ntau: DF Tsawg dua lossis sib npaug ntawm 0.3 MPa·cm² / g

Qib zaj duab xis / txhaj tshuaj: DF Tsawg dua lossis sib npaug ntawm 0.6 MPa·cm² / g

⑤ Migration Resistance & Huab cua ceev

Lub teeb- cov khoom xim muaj xim yuav tsum tau kuaj kev tsiv teb tsaws (kev sib cuag thiab hnyav tsiv teb tsaws)

Cov khoom siv sab nraum zoov: huab cua ceev ntau dua lossis sib npaug rau Qib 4 (ib ISO 105-B02)

Kev sib cuag zaub mov: daim ntawv pov thawj kev ua raws cai (FDA, EFSA, GB 9685)

3. Daim Ntawv Thov -Kev Qhia Txog Kev Xaiv Tshwj Xeeb

Daim ntawv thov

Tus neeg nqa khoom

Chaw thau khoom

Thaum tshav kub kub Resistance

Ntsiab tsom

Txhaj Moulded Housewares

Homo-PP MFI 20 ~ 30

2%~3%

Ntau dua lossis sib npaug li 240 degree

Xim brightness, gloss, tsis muaj migration

Blown Film / Cast Film

Co-PP MFI 8~15

1.5%~2.5%

Ntau tshaj lossis sib npaug li 230 degree

Zaj duab xis uniformity, tensile zog

Nonwoven / Fiber ntau

Homo-PP MFI Ntau dua lossis sib npaug rau 35

1%~2%

Ntau dua lossis sib npaug li 260 degree

Tsawg lim tus nqi, kev nyab xeeb ntawm daim tawv nqaij

Cov kav dej / Cov khoom siv sab nrauv

Co-PP cuam tshuam- hloov kho

2%~4%

Ntau dua lossis sib npaug li 260 degree

Huab cua ceev Ntau dua lossis sib npaug li 4, UV tsis kam

Khoom noj khoom haus tiv tauj

Khoom noj khoom haus- qib PP

Tsawg dua lossis sib npaug li 2%

Ntau dua lossis sib npaug li 240 degree

Migration test, FDA daim ntawv pov thawj

4. Cov lus nug uas nquag nug

Q: Xim me ntsis ntawm kev txhaj tshuaj molded qhov chaw. Ua rau?

Feem ntau tsis zoo masterbatch dispersion. Kev daws: ① Ua kom rov qab siab (5 ~ 10 MPa); ② tsa qhov kub thiab txias los ntawm 10 ~ 15 degree; ③ Hloov mus rau masterbatch nrog kev ua haujlwm zoo dua.

Q: Cov xim tseem ceeb sib txawv ntawm cov khoom siv. Yuav tswj li cas?

Thov batch-los ntawm-batch xim txawv daim ntawv qhia (ΔE tus nqi). Kev lees paub tus qauv: ΔE Tsawg dua lossis sib npaug rau 1.0. Saib xyuas tus neeg xa khoom zoo ib yam, qauv, thiab kev yuav khoom batch.

Q: Cov khoom ua nkig tom qab ntxiv masterbatch. Vim li cas?

Tej yam ua tau: ① Cov khoom thauj khoom tsis sib xws; ② Kev thauj khoom ntau dhau; ③ Cov tshuaj dispersants tsis sib xws lossis siv quav ciab. Txo kev thauj khoom thiab hloov mus rau cov cab kuj sib xws.

Q: Dawb PP khoom tig daj. Ua rau?

① TiO₂ qib tsis raug - siv Rutile-hom (R- qib) TiO₂; ② Ua haujlwm kub dhau ua rau PP thermal degradation; ③ Fluorescent whitening agents uas tsis muaj cua sov tsis txaus.

5. Cov ntaub ntawv thov ua ntej yuav khoom

Cov ntaub ntawv

Lub hom phiaj

TDS (Technical Data Sheet)

Txheeb xyuas MFI, hom cab kuj, cov ntsuas kub tsis kam

COA (Certificate of Analysis)

Paub meej batch-rau-batch zoo sib xws

MSDS/SDS (Safety Data Sheet)

Nkag siab txog cov ntaub ntawv kev nyab xeeb ntawm cov khoom

Filter Pressure Value Report

Ntsuam xyuas cov qib zoo dispersion

Huab cua ceev Test Report

Yuav tsum tau rau cov khoom siv sab nraum zoov

FDA / EU Daim Ntawv Pov Thawj Ua Raws Cai

Yuav tsum tau rau cov khoom noj khoom haus

RoHS / REACH Tshaj Tawm

Yuav tsum tau rau EU export khoom

6. Cov ntsiab lus

Lub hauv paus ntsiab lus tseem ceeb: cov cab kuj sib xws, sib tw MFI, txaus tshav kub tsis kam, zoo heev dispersion, thiab ua tiav cov ntaub ntawv ua raws. Cov kev xav tau sib txawv los ntawm kev ua tiav thiab xaus - siv daim ntawv thov. Ib txwm ua me me -batch sim ntau lawm ua ntej tag nrho -scale procurement.

Xa kev nug